{"id":5338,"date":"2026-10-03T22:47:52","date_gmt":"2026-10-03T14:47:52","guid":{"rendered":"https:\/\/www.corvelanmag.com\/?p=5338"},"modified":"2026-11-16T18:47:09","modified_gmt":"2026-11-16T10:47:09","slug":"scrap-metal-magnetic-separation","status":"publish","type":"post","link":"https:\/\/www.corvelanmag.com\/ru\/scrap-metal-magnetic-separation\/","title":{"rendered":"\u041e\u0447\u0438\u0441\u0442\u043a\u0430 \u043b\u043e\u043c\u0430 \u043f\u043e\u0441\u043b\u0435 \u043f\u0440\u0435\u0441\u0441-\u043d\u043e\u0436\u043d\u0438\u0446: \u0443\u0434\u0430\u043b\u0435\u043d\u0438\u0435 \u0440\u0435\u0437\u0438\u043d\u044b \u0438 \u0442\u0435\u043a\u0441\u0442\u0438\u043b\u044f"},"content":{"rendered":"\n<style>\n.cv-shear { --cs-ink:#182b3b; --cs-link:#155a7e; --cs-edge:#ccdce4; --cs-bg:#f4f8fa; max-width:1400px; width:100%; margin-inline:auto; padding-inline:clamp(16px,3vw,42px); box-sizing:border-box; color:var(--cs-ink); line-height:1.67; font-size:clamp(16px,1.3vw,18px); overflow-wrap:anywhere; }\n.cv-shear h2,.cv-shear h3 { color:var(--cs-ink); line-height:1.24; }\n.cv-shear h2 { font-size:clamp(24px,3.3vw,36px); margin:0 0 16px; scroll-margin-top:105px; }\n.cv-shear h3 { font-size:clamp(19px,2.3vw,26px); margin:25px 0 10px; }\n.cv-shear p { margin:0 0 14px; }\n.cv-shear section { display:block; margin-block:clamp(32px,5vw,58px); }\n.cv-shear .cs-lead { font-size:clamp(18px,1.65vw,22px); margin:0 0 23px; }\n.cv-shear a { color:var(--cs-link); text-decoration:underline; text-underline-offset:.18em; }\n.cv-shear a:hover { text-decoration-thickness:2px; }\n.cv-shear a:focus-visible,.cv-shear summary:focus-visible,.cv-shear .cs-table:focus-visible { outline:3px solid #1273a0; outline-offset:3px; }\n.cv-shear .cs-toc { display:block; padding:18px clamp(16px,3vw,30px); border:1px solid var(--cs-edge); border-left:4px solid #2c6b85; background:var(--cs-bg); border-radius:6px; }\n.cv-shear .cs-toc p { font-weight:700; margin-bottom:7px; }\n.cv-shear .cs-toc ol { margin:0; padding-inline-start:1.5em; }\n.cv-shear .cs-toc li { margin-bottom:4px; }\n.cv-shear .cs-media { display:block; margin:0 0 18px; width:100%; }\n.cv-shear .cs-media img { display:block; width:auto; max-width:100%; height:auto; border-radius:6px; }\n.cv-shear .cs-table { display:block; max-width:100%; overflow-x:auto; margin:18px 0; }\n.cv-shear table { width:100%; min-width:510px; border-collapse:collapse; font-size:.96em; }\n.cv-shear th,.cv-shear td { border:1px solid var(--cs-edge); padding:10px 12px; text-align:left; vertical-align:top; }\n.cv-shear th { background:#e9f2f6; }\n.cv-shear .cs-faq details { border-top:1px solid var(--cs-edge); padding:12px 0; }\n.cv-shear .cs-faq details:last-child { border-bottom:1px solid var(--cs-edge); }\n.cv-shear .cs-faq summary { cursor:pointer; font-weight:700; }\n.cv-shear .cs-faq details p { margin:9px 0 0; }\n.cv-shear .cs-button { display:inline-block; margin-top:12px; padding:9px 14px; border-radius:5px; color:#fff; background:#155a7e; font-weight:700; text-decoration:none; }\n.cv-shear .cs-button:hover { background:#104762; }\n@media (max-width:600px) {\n  .cv-shear { padding-inline:16px; }\n  .cv-shear section { margin-block:34px; }\n  .cv-shear th,.cv-shear td { padding:8px 9px; }\n}\n<\/style>\n<article class=\"cv-shear\" lang=\"en-US\">\n<p class=\"cs-lead\"><strong>To clean steel scrap after a shear, spread the feed, magnetically recover the steel, and give loose rubber and textiles a separate discharge path.<\/strong> If dirt or fabric is trapped between steel pieces, improve feed presentation and test a scrap drum that turns the steel as it travels. If rubber is bolted on, molded around a frame, or pinched inside folded steel, set those pieces aside for mechanical release and re-sort them. In shear scrap magnetic cleaning, that distinction tells you whether to adjust the line or change how you prepare the scrap.<\/p><nav aria-label=\"On this page\" class=\"cs-toc\" data-article-section=\"navigation\"><p>On this page<\/p><ol>\n<li><a href=\"#how-it-works\">How Does Magnetic Cleaning Work After a Scrap Shear?<\/a><\/li>\n<li><a href=\"#inspect-feed\">How Can You Tell Why Rubber and Textiles Are Still in the Steel?<\/a><\/li>\n<li><a href=\"#meter-and-screen\">How Should You Feed and Screen Scrap After the Shear?<\/a><\/li>\n<li><a href=\"#choose-magnet\">Should You Use a Magnetic Drum or an Overband Magnet?<\/a><\/li>\n<li><a href=\"#loose-carryover\">What Should You Change if Loose Fabric Still Reaches the Steel Bin?<\/a><\/li>\n<li><a href=\"#attached-material\">How Do You Handle Rubber or Textiles Still Attached to Steel?<\/a><\/li>\n<li><a href=\"#reject-stream\">What Should You Do With the Material the Magnet Leaves Behind?<\/a><\/li>\n<li><a href=\"#buyer-spec\">How Do You Define Clean Enough for the Steel Buyer?<\/a><\/li>\n<li><a href=\"#trial\">How Do You Test a Post-Shear Cleaning Line?<\/a><\/li>\n<li><a href=\"#retrofit\">What Should You Check Before Retrofitting a Shear-Scrap Line?<\/a><\/li>\n<li><a href=\"#next-step\">Start With the Material That Still Follows the Steel<\/a><\/li>\n<li><a href=\"#faq\">Frequently Asked Questions<\/a><\/li>\n<\/ol><\/nav>\n<section>\n<h2 id=\"how-it-works\">How Does Magnetic Cleaning Work After a Scrap Shear?<\/h2>\n<p><strong>A magnet pulls the steel into a separate stream, leaving free rubber, textiles, and other nonmagnetic pieces to follow the ordinary discharge path.<\/strong> A practical starting layout is shear discharge \u2192 metered feed \u2192 optional screen \u2192 magnetic steel recovery \u2192 separate steel and reject chutes. Put the collection points where neither stream can bounce back into the other.<\/p>\n<h3>What actually moves toward the magnet?<\/h3>\n<p><strong>Iron and magnetically responsive steel are the parts the magnet picks up.<\/strong> A loose seat-cover fragment can fall away, while a rubber mount with a steel bracket moves as one piece if the magnet captures the bracket. This is why you can recover steel successfully and still have enough rubber or fabric in the product to fail a buyer\u2019s check.<\/p>\n<h3>How does shear scrap differ from shredded scrap?<\/h3>\n<p><strong>Post-shear feed can contain large, bent or folded pieces with attachments still on them.<\/strong> A line built around a finer shredded stream may need a different feeder, opening and transfer path to handle those pieces. <a href=\"https:\/\/steinertglobal.com\/us\/applications\/metal-recycling\/shear-scrap\/\" rel=\"nofollow noopener\" target=\"_blank\">STEINERT\u2019s shear-scrap application<\/a> describes a line with a screen, a purpose-configured electromagnetic drum and optional nonferrous recovery. Use that as a process reference and test your actual size range before specifying equipment.<\/p>\n<\/section>\n<section>\n<h2 id=\"inspect-feed\">How Can You Tell Why Rubber and Textiles Are Still in the Steel?<\/h2>\n<p><strong>Sort the contamination in a safely collected steel sample by how it stays with the metal.<\/strong> Check for all three in each trial. They can appear together in a single bin and call for different changes. Track the mass in each group where you can separate it safely and keep intact composites in their own category until they are assayed.<\/p>\n<h3>Is it loose, trapped, or attached?<\/h3>\n<p><strong>Watch what happens when pieces are separated in a designated inspection area.<\/strong> Use the table to choose the first trial. Photograph intact assemblies so a repeating source, such as steel-backed rubber mounts, can be traced to the incoming lot.<\/p>\n<div aria-label=\"Contamination diagnosis\" class=\"cs-table\" role=\"region\" tabindex=\"0\"><table><thead><tr><th scope=\"col\">What you find<\/th><th scope=\"col\">What it suggests<\/th><th scope=\"col\">What to try first<\/th><\/tr><\/thead><tbody>\n<tr><td>Loose strips or fabric lying among recovered steel<\/td><td>Parts traveled together or the streams mixed after discharge<\/td><td>Spread the feed and inspect the splitter and chutes<\/td><\/tr>\n<tr><td>Fabric comes free after a steel pile or nested pieces are separated<\/td><td>Steel was physically carrying loose material<\/td><td>Test a shallower bed and controlled turnover<\/td><\/tr>\n<tr><td>Rubber stays bolted to steel or fabric stays pinched in a fold<\/td><td>The materials are still joined<\/td><td>Divert the composite for separate release and re-sorting<\/td><\/tr>\n<\/tbody><\/table><\/div>\n<h3>What should you record about the feed?<\/h3>\n<p><strong>Record piece length, width and shape alongside the usual size range, moisture and peak feed rate.<\/strong> A long strap or bent plate can bridge an opening that handles ordinary pieces of similar weight. Track the steel, loose rubber, textiles, fines and any nonferrous pieces by incoming lot. Keep wet or heavily tangled lots identifiable so their results do not disappear into an average.<\/p>\n<\/section>\n<section>\n<h2 id=\"meter-and-screen\">How Should You Feed and Screen Scrap After the Shear?<\/h2><div class=\"cs-media\"><img loading=\"lazy\" alt=\"How Should You Feed and Screen Scrap After the Shear?\" decoding=\"async\" height=\"800\" loading=\"lazy\" src=\"https:\/\/www.corvelanmag.com\/wp-content\/uploads\/2026\/11\/scrap-recycling-conveyor-feeder-wide-1-1-1-1-1.webp\" width=\"1200\"\/><\/div>\n<p><strong>Use a feeder sized for the largest allowed pieces to turn intermittent shear drops into a steady, spread-out feed.<\/strong> Evaluate a screen when undersize is a distinct fraction you can handle and test separately. The goal is to give steel and loose contaminants room to follow different paths.<\/p>\n<h3>How do you control surges from the shear?<\/h3>\n<p><strong>Meter the discharge and check the deepest part of the bed during an actual shear cycle.<\/strong> A feeder can keep one charge from landing on top of another at the pickup point. If dirty product appears right after each drop, compare a controlled feed window with a normal surge window. Hold the scrap lot and separator settings steady. If the shallower feed helps, test whether the feeder can maintain that profile at the required throughput.<\/p>\n<h3>When is a screen worth adding?<\/h3>\n<p><strong>Test a screen when dirt, small rubber chips or other fines crowd the main sorting stage.<\/strong> Keep the undersize in a separate bin and assay it for small steel before deciding where it goes. Where flat plates cover openings or fabric wraps around screen components, check the screen\u2019s ability to keep working under actual loads. The steel content and added stoppages tell you whether to change the cut, add a fines recovery step, or keep the feed on one path. Choose the opening from measured size fractions and an actual trial. A cut that removes plenty of dirt can still be a poor choice if it diverts the small steel you sell.<\/p>\n<\/section>\n<section>\n<h2 id=\"choose-magnet\">Should You Use a Magnetic Drum or an Overband Magnet?<\/h2>\n<p><strong>Start with a scrap-rated drum for controlled pickup and cleaning at a transfer. Consider an overband for bulk steel pickup above an existing belt.<\/strong> The choice depends on the largest and hardest-to-lift pieces, the depth of material at the magnet, and whether the recovered steel needs to turn over before discharge.<\/p>\n<h3>When does a drum do the better cleaning job?<\/h3><div class=\"cs-media\"><img loading=\"lazy\" alt=\"When does a drum do the better cleaning job?\" decoding=\"async\" height=\"900\" loading=\"lazy\" src=\"https:\/\/www.corvelanmag.com\/wp-content\/uploads\/2026\/11\/magnetic-drum-ferrous-separation-operation-2-1-1-1-1.webp\" width=\"1200\"\/><\/div>\n<p><strong>Use a drum when the line can deliver a controlled bed across the working width and the shell, chutes and drive can handle the impact.<\/strong> Ask the supplier where the steel is picked up, where it turns, and where it releases. <a href=\"https:\/\/www.eriez.com\/Products\/Metals-Recycling\/Ferrous-Recovery\/Magnetic-Scrap-Drums\" rel=\"nofollow noopener\" target=\"_blank\">Eriez\u2019s scrap drum documentation<\/a> distinguishes agitating drums that help shed loose contaminants from transfer drums designed to carry the steel through. If your feed is regular and free-flowing, our <a href=\"https:\/\/www.corvelanmag.com\/products\/dry-drum-magnetic-separator\/\">dry drum magnetic separator<\/a> page can help you check the feed and installation requirements. Submit the largest pieces and impact conditions so we can assess whether the dry bulk design fits your duty. Specify whether the material falls directly on the drum or reaches it on a controlled trajectory. The impact at the shell can change what frame, liner and feed arrangement the installation needs.<\/p>\n<h3>When does an overband fit an existing belt?<\/h3>\n<p><strong>Consider an overband when you can lift the target steel from the conveyor and discharge it into its own chute.<\/strong> Measure belt width, speed, maximum bed depth and the space between the magnet and the belt. Also check the clear route from the pickup zone to the steel bin. On a belt full of heavy, overlapping pieces, verify pickup under peak conditions and check the steel bin for carryover. See our <a href=\"https:\/\/www.corvelanmag.com\/products\/overband-magnetic-separator\/\">overband magnetic separator<\/a> page for crossbelt and inline layouts and the conveyor data used to evaluate them.<\/p>\n<\/section>\n<section>\n<h2 id=\"loose-carryover\">What Should You Change if Loose Fabric Still Reaches the Steel Bin?<\/h2>\n<p><strong>Find out whether the fabric was lifted with steel or entered the steel chute after the split.<\/strong> Keep the feed source and rate comparable while you change one condition. Check the reject for missed steel so a cleaner product does not come at the expense of too much recovery.<\/p>\n<h3>When does turning the steel help?<\/h3>\n<p><strong>Turnover can release loose material held under or between pieces.<\/strong> A scrap drum with agitating poles can turn suitable steel as it travels around the shell, giving the material another chance to fall away. When big pieces dominate or steel drops early, evaluate the pickup and release behavior first. <a href=\"https:\/\/www.eriez.com\/Documents\/Literature\/Data-Sheet\/Recycling\/MRB-112-Scrap-Cleaner_DS.pdf\" rel=\"nofollow noopener\" target=\"_blank\">Eriez\u2019s scrap cleaner data sheet<\/a> illustrates the trade-off between agitating poles and radial poles for larger, harder-to-handle scrap.<\/p>\n<h3>When should you inspect the splitter and chutes?<\/h3>\n<p><strong>If the streams look separate as they leave the magnet but the bin stays dirty, inspect the downstream transfer.<\/strong> Look from a safe observation point for bouncing chunks, a chute that backs up, or fabric dropping into the wrong bin. If a splitter change helps appearance, weigh and sort the reject from the same interval. A splitter can shift borderline pieces to reject, including steel you meant to keep. Compare the reject at steady feed and during peak shear drops. Steel lost mainly during peaks points first to feed delivery. Loss at both rates calls for a closer look at the pickup point, magnetic configuration and discharge geometry.<\/p>\n<\/section>\n<section>\n<h2 id=\"attached-material\">How Do You Handle Rubber or Textiles Still Attached to Steel?<\/h2>\n<p><strong>Divert persistent composites and free the attachment before you sort again.<\/strong> Choose a release method that suits the assembly and the site\u2019s safe handling procedures. A stronger magnet may pick up more of both materials when they move as one piece.<\/p>\n<h3>Which pieces belong in a separate rework stream?<\/h3>\n<p><strong>Set aside pieces that stay joined through normal transfer and turnover.<\/strong> Common trial categories include rubber with a steel backing, strips crimped inside folded sheet and fabric wrapped tightly around steel wire. Record the weight and source of the composites. A repeated part from one supplier may be easier to remove before the shear or handle as a separate batch. A spread across many lots may make a dedicated rework path more practical. Match the method to the joint. For example, an impact or tumbling trial may release packed dirt from compatible scrap, while a bolted rubber mount needs a process that can physically separate the parts. Inspect the steel and rework residue afterward to see what came free.<\/p>\n<h3>When is a second magnetic pass useful?<\/h3>\n<p><strong>Test a second pass when the first stage leaves valuable free steel in the reject or loose contamination in the steel.<\/strong> These are different duties. A recovery pass treats the reject to pick up missed steel. A cleaning pass treats the magnetic product after spreading or turning it. Sample the stream that the second stage would actually treat. If intact attachments dominate, compare rework with another pass before adding equipment.<\/p>\n<\/section>\n<section>\n<h2 id=\"reject-stream\">What Should You Do With the Material the Magnet Leaves Behind?<\/h2>\n<p><strong>Check the reject for lost steel first, then choose a downstream process for a fraction you can actually recover.<\/strong> A reject stream may contain rubber, textile fluff, fines, free nonferrous pieces and some steel. How those materials are distributed by size and shape matters more than the total reject tonnage on its own.<\/p>\n<h3>Can an air separator take out rubber and textiles?<\/h3>\n<p><strong>Air separation is worth testing for dry, loose material with a repeatable difference in how readily it moves in air.<\/strong> <a href=\"https:\/\/nihot.nl\/products\/wsv-wsz-windshifter\/\" rel=\"nofollow noopener\" target=\"_blank\">Nihot\u2019s windshifter documentation<\/a> describes light and heavy splits for recycling streams. In your feed, wet fabric, dense rubber and flat metal can complicate that split. Try size fractions separately, weigh steel lost in the light stream, and plan for dust collection and the space needed to handle residues.<\/p>\n<h3>When is eddy current separation worth a trial?<\/h3>\n<p><strong>Trial an eddy current separator when the prepared reject contains enough free, conductive nonferrous metal to justify recovery.<\/strong> Size and spread the feed for the separator and confirm the upstream ferrous cleanup requirements with its supplier. Free aluminum can be a recovery target. Check metal mass in the separate recovered fraction and residual reject so that a heavier discharge full of rubber does not get counted as better metal recovery. Rubber with metal embedded in it remains a composite and needs its own evaluation. For a broader view of how the ferrous and reject streams fit into the yard, see our <a href=\"https:\/\/www.corvelanmag.com\/applications\/scrap-metal-separation\/\">scrap metal separation applications<\/a>.<\/p>\n<\/section>\n<section>\n<h2 id=\"buyer-spec\">How Do You Define Clean Enough for the Steel Buyer?<\/h2>\n<p><strong>Ask for the buyer\u2019s written grade, contaminant limits, inspection method and terms for off-spec loads before setting the line target.<\/strong> Start with the agreed grade and ask how the buyer treats rubber, textiles, dirt, attachments and oversized pieces. <a href=\"https:\/\/www.isrispecs.org\/wp-content\/uploads\/2026\/01\/2026-January-ReMA_ISRI_Specifications.pdf\" rel=\"nofollow noopener\" target=\"_blank\">ReMA\u2019s ISRI Specifications<\/a> list ferrous grades including heavy melting steel. Use the applicable grade and the receiver\u2019s purchase terms to set the trial criteria.<\/p>\n<h3>What needs to be on the acceptance sheet?<\/h3>\n<p><strong>Define what counts as a contaminant and how its weight will be measured.<\/strong> Agree on the sample point, sample method, size or piece limits, and whether results are reported as received or on a dry basis. Record whether attachments are counted by total composite mass or by their nonsteel portion. Decide who can release, hold, blend or rework an off-spec lot under the purchase agreement.<\/p>\n<h3>How do purity and recovery tell different stories?<\/h3>\n<p><strong>Steel purity tells you what is in the product. Steel recovery tells you how much of the incoming steel made it there.<\/strong> Calculate purity as steel mass in the product \u00f7 total product mass \u00d7 100. Calculate recovery as steel mass in the product \u00f7 steel mass in the feed \u00d7 100. If the buyer caps specific contaminants, report their mass fractions or counts separately. A single purity number can hide which material caused the failure.<\/p>\n<\/section>\n<section>\n<h2 id=\"trial\">How Do You Test a Post-Shear Cleaning Line?<\/h2>\n<p><strong>Compare the baseline with one defined change at a time and account for the mass and steel content of every output over the same feed window.<\/strong> Pick comparable lots and meet the rate your yard needs. During each run, log surges, interruptions and any material still held in the equipment at the end.<\/p>\n<h3>Where should you weigh and sample?<\/h3>\n<p><strong>Collect representative samples from the incoming feed, steel product and each reject, oversize or fines stream through designated safe collection points.<\/strong> Use timed samples with the transport delay accounted for or isolate and clear a measured trial lot. Keep one weight basis for every stream. Record feed rate, bed depth, size range and settings alongside the weights. If the balance does not close within your agreed weighing and sampling allowance, locate the missing stream or retained material before comparing results.<\/p>\n<h3>What does a balanced trial tell you?<\/h3>\n<p><strong>A mass balance can show that a cleaner-looking load still sends too much steel to reject.<\/strong> In this illustrative 1,000 kg dry-basis lot, the feed contains 800 kg of steel. Assume the three measured outputs account for the full lot and report the steel contained in any composites separately during the assay.<\/p>\n<div aria-label=\"Illustrative mass balance\" class=\"cs-table\" role=\"region\" tabindex=\"0\"><table><thead><tr><th scope=\"col\">Output<\/th><th scope=\"col\">Total mass (kg)<\/th><th scope=\"col\">Steel (kg)<\/th><th scope=\"col\">Other material (kg)<\/th><\/tr><\/thead><tbody>\n<tr><td>Steel product<\/td><td>780<\/td><td>760<\/td><td>20<\/td><\/tr><tr><td>Main reject<\/td><td>160<\/td><td>25<\/td><td>135<\/td><\/tr><tr><td>Screen undersize<\/td><td>60<\/td><td>15<\/td><td>45<\/td><\/tr><tr><th scope=\"row\">Total measured output<\/th><td>1,000<\/td><td>800<\/td><td>200<\/td><\/tr>\n<\/tbody><\/table><\/div>\n<p>The product is 760 \u00f7 780 = <strong>97.4% steel by mass<\/strong>, while steel recovery is 760 \u00f7 800 = <strong>95.0%<\/strong>. There are 40 kg of steel outside the product. The main reject contains more lost steel by mass, but the undersize is richer in steel at 25.0%, versus 15.6% in the main reject. If purity meets the agreed limit but recovery falls short, compare the recoverable steel and cost of treating each stream. If purity falls short, sort the product contaminants first and repeat the trial at the intended operating rate.<\/p>\n<\/section>\n<section>\n<h2 id=\"retrofit\">What Should You Check Before Retrofitting a Shear-Scrap Line?<\/h2>\n<p><strong>Measure the existing transfer and discharge space before selecting a separator, then price the installed line against the required saleable output.<\/strong> Include the feeder or screen, chutes, collection space, guards and service access in the comparison. For a retrofit, turn trial results into saleable steel tons per operating hour. Compare the buyer\u2019s price or deduction, recovered byproducts, residue disposal, power and labor at the same feed basis. Recurring stoppages can erase a saving that looks attractive in the equipment quote. A machine that fits the belt can still lack a workable route to discharge or clear large pieces.<\/p>\n<h3>Which operating problems should the layout account for?<\/h3>\n<p><strong>Provide safe inspection points and access to clear jams or textile wrap under the site\u2019s energy-control procedure.<\/strong> Plan for sharp scrap, heavy falling pieces and flyout at transfers. Where dust, drop noise or carryback affects operation, check that guards or enclosures, extraction where applicable, and cleanup access fit the layout together. For U.S. operations, see <a href=\"https:\/\/www.osha.gov\/laws-regs\/regulations\/standardnumber\/1910\/1910.147\" rel=\"nofollow noopener\" target=\"_blank\">OSHA\u2019s hazardous energy standard<\/a> for covered servicing. Use your applicable local rules and machine-specific procedure, including the residual attraction of permanent magnets.<\/p>\n<h3>What should you send for an equipment review?<\/h3>\n<p><strong>Send a drawing of the shear discharge and available transfer, feed photos with a scale, the usual and maximum piece sizes, normal and peak throughput, and your buyer\u2019s acceptance target.<\/strong> For a belt installation, add width, speed and maximum bed depth. Include photos or measured weights of the contamination in each stream if available. We can review your feed, candidate magnetic stages and installation interfaces. <a class=\"cs-button\" href=\"https:\/\/www.corvelanmag.com\/contact-us\/\">Send Corvelan your scrap and line details<\/a><\/p>\n<\/section>\n<section data-article-section=\"conclusion\">\n<h2 id=\"next-step\">Start With the Material That Still Follows the Steel<\/h2>\n<p>When loose rubber or fabric reaches the steel bin, start with feed presentation, turnover and chute separation. When material stays attached, set up a separate release and re-sort step. Use the buyer\u2019s agreed limits and the steel measured in both product and reject to decide whether the change earns a place on the line.<\/p>\n<\/section>\n\n<section class=\"cs-faq\" data-article-section=\"faq\">\n<h2 id=\"faq\">Frequently Asked Questions<\/h2>\n<details><summary>Can I process rain-soaked shear scrap and dry scrap together?<\/summary><p>Run them as separate trial lots first. Wet fabric can cling to steel or clump with fines, so a dry-lot result may overstate performance on wet feed. If both are part of normal production, agree on a sampling and weight basis for each condition.<\/p><\/details>\n<details><summary>Why does a bundle of textile fluff stick to the magnet?<\/summary><p>Look for steel wire, clips or other magnetic pieces inside a safely collected bundle. The magnet can pick up the steel and lift the attached fluff with it. Track those bundles separately to see whether a wire-rich feed source needs different preparation.<\/p><\/details>\n<details><summary>Why do thin plates cause trouble even when they are light?<\/summary><p>Thin plates can bridge a chute, overlap at the pickup point or cover a screen opening. Give the supplier dimensions and photos of the longest pieces in their usual orientation. Include those pieces in the trial to see how they travel through the entire transfer.<\/p><\/details>\n<details><summary>What capacity figure should I ask a supplier to guarantee?<\/summary><p>Ask for a feed rate with a stated feed envelope, operating pattern, sampling method, product limit and minimum steel recovery. Agree on steady running and peak shear discharge separately. A tonnes-per-hour figure by itself leaves both cleanliness and yield undefined.<\/p><\/details>\n<details><summary>Can I compare one grab sample from each bin?<\/summary><p>Take repeated increments over the same feed window. One scoop from the top of a bin can miss heavy steel at the bottom or fluff that collected on one side. Include startup or end-of-run material separately if it is part of what you normally ship.<\/p><\/details>\n<details><summary>How should I compare suppliers when my scrap comes from several sources?<\/summary><p>Give each supplier comparable lots that represent your normal mix and a difficult lot you expect to run. Request results by lot so a clean run cannot mask losses or contamination on the tougher feed.<\/p><\/details>\n<details><summary>When does a manual picking station make sense?<\/summary><p>Consider a guarded, purpose-designed picking station if a small share of large, recognizable pieces repeatedly causes a shipment to fail. Assess exposure to sharp pieces, falling material and moving equipment before choosing a station. For frequent or hard-to-identify attachments, compare mechanical rework or upstream segregation.<\/p><\/details>\n<details><summary>Can I return screen undersize straight to the steel product?<\/summary><p>Return it only if the buyer accepts that fraction and the blended lot still meets the grade. Otherwise, keep undersize segregated, measure the recoverable steel, and trial a separate recovery step before deciding whether to blend anything.<\/p><\/details>\n<details><summary>Why do our contamination numbers disagree with the mill\u2019s?<\/summary><p>Compare sampling location, lot definition, moisture basis and how each side counted intact assemblies. Then inspect or split a shared sample under an agreed method. This helps you tell whether the mismatch comes from the process or from two different inspection rules.<\/p><\/details>\n<details><summary>What should I check after a textile-wrap stoppage?<\/summary><p>Follow your site\u2019s isolation, clearing and restart procedures. After authorized restart, verify feed distribution and collect steel and reject samples through the designated points. A cleared blockage can restore flow while a shifted splitter or recurrent wrap still affects product quality.<\/p><\/details>\n<\/section>\n<script type=\"application\/ld+json\">\n{\n  \"@context\": \"https:\/\/schema.org\",\n  \"@type\": \"FAQPage\",\n  \"mainEntity\": [\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Can I process rain-soaked shear scrap and dry scrap together?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Run them as separate trial lots first. Wet fabric can cling to steel or clump with fines, so a dry-lot result may overstate performance on wet feed. If both are part of normal production, agree on a sampling and weight basis for each condition.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Why does a bundle of textile fluff stick to the magnet?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Look for steel wire, clips or other magnetic pieces inside a safely collected bundle. The magnet can pick up the steel and lift the attached fluff with it. Track those bundles separately to see whether a wire-rich feed source needs different preparation.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Why do thin plates cause trouble even when they are light?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Thin plates can bridge a chute, overlap at the pickup point or cover a screen opening. Give the supplier dimensions and photos of the longest pieces in their usual orientation. Include those pieces in the trial to see how they travel through the entire transfer.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"What capacity figure should I ask a supplier to guarantee?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Ask for a feed rate with a stated feed envelope, operating pattern, sampling method, product limit and minimum steel recovery. Agree on steady running and peak shear discharge separately. A tonnes-per-hour figure by itself leaves both cleanliness and yield undefined.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Can I compare one grab sample from each bin?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Take repeated increments over the same feed window. One scoop from the top of a bin can miss heavy steel at the bottom or fluff that collected on one side. Include startup or end-of-run material separately if it is part of what you normally ship.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"How should I compare suppliers when my scrap comes from several sources?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Give each supplier comparable lots that represent your normal mix and a difficult lot you expect to run. Request results by lot so a clean run cannot mask losses or contamination on the tougher feed.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"When does a manual picking station make sense?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Consider a guarded, purpose-designed picking station if a small share of large, recognizable pieces repeatedly causes a shipment to fail. Assess exposure to sharp pieces, falling material and moving equipment before choosing a station. For frequent or hard-to-identify attachments, compare mechanical rework or upstream segregation.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Can I return screen undersize straight to the steel product?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Return it only if the buyer accepts that fraction and the blended lot still meets the grade. Otherwise, keep undersize segregated, measure the recoverable steel, and trial a separate recovery step before deciding whether to blend anything.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Why do our contamination numbers disagree with the mill\u2019s?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Compare sampling location, lot definition, moisture basis and how each side counted intact assemblies. Then inspect or split a shared sample under an agreed method. This helps you tell whether the mismatch comes from the process or from two different inspection rules.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"What should I check after a textile-wrap stoppage?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Follow your site\u2019s isolation, clearing and restart procedures. After authorized restart, verify feed distribution and collect steel and reject samples through the designated points. A cleared blockage can restore flow while a shifted splitter or recurrent wrap still affects product quality.\"\n      }\n    }\n  ]\n}\n<\/script>\n<\/article>\n","protected":false},"excerpt":{"rendered":"<p>To clean steel scrap after a shear, spread the feed, magnetically recover the steel, and give loose rubber and textiles a separate discharge path. If dirt or fabric is trapped between steel pieces, improve feed presentation and test a scrap drum that turns the steel as it travels. If rubber is bolted on, molded around [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":4025,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"footnotes":""},"categories":[1],"tags":[],"class_list":["post-5338","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-blog"],"acf":[],"_links":{"self":[{"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/posts\/5338","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/comments?post=5338"}],"version-history":[{"count":5,"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/posts\/5338\/revisions"}],"predecessor-version":[{"id":6141,"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/posts\/5338\/revisions\/6141"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/media\/4025"}],"wp:attachment":[{"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/media?parent=5338"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/categories?post=5338"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.corvelanmag.com\/ru\/wp-json\/wp\/v2\/tags?post=5338"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}